RestrictViewTM laminated security glass enables the viewer to see through one piece of glass, but not through two pieces.
|
|
RestrictViewTM Laminated Glass
Product Description
RestrictViewTM glass is designed to prevent viewing through two pieces of glass while it permits viewing through one piece. This means, for example, that in a hospital, patients can see nurses or attendants in the corridor through windows in their rooms, and the nurses can see the patients. Patients, however, cannot see across the corridor into the room of another patient. In a courtyard application, people can see into the courtyard, but cannot see through to viewers on the other side. Adjoining treatment rooms or conference rooms are only viewable from corridors.
RestrictViewTM glass is a laminate and can be manufactured in a variety of formats, including approved attack specification formats for psychiatric hospitals and prisons.
Product Specifications
Make-up:
4.76 mm (3/16”) make-up comprising:
4-mm SCHOTT AMIRAN® anti-reflective glass
0.76-mm polyurethane with RV interlayer
4-mm SCHOTT AMIRAN® anti-reflective glass
Average thickness: 4.76 mm (3/16”)Weight: 4.68 lbs/ft2
Maximum dimensions: 44” x 44”
Applications:
Corridors
Hospitals
Prisons
Courtyards
Conference rooms
Wherever restricted vision into adjoining glass-enclosed
spaces is desired
For additional information, please contact:
Advanced Materials
SCHOTT North America, Inc.
555 Taxter Road
Tel: (914) 831-2240
Fax: (914) 831-2346
Elmsford, NY 10523
architecture@us.schott.com
www.us.schott.com/architecture
|
RestrictView Data Sheet
|
|