PERFORMANCE DATA


Notes: 1. 380-2780 nm (nanometers) according to DIN 678507 2. According to DIN 67507 3. Shading coefficient according to DIN 2078 4. According to DIN 6169 5. Data applies to wavelengths of 320 to 2500 nm 6. According to DIN 4108

Product is available as:
  • Tempered safety glass
  • Laminated safety glass
  • Insulated glass units
  • Low-iron glass (water-white glass)
  • Low-E glass
  • UV-blocking glass (98% UV absorption)

Maximum dimensions: 69" x 147"
Thicknesses: 5/32"; 1/4"; 3/8"; 1/2"
Residual reflection (90º angle):
As little as 1% with single glazing and laminated safety glass; as little as 2% with double glazing when both panes are AMIRAN.

Color of residual reflection:
Unobtrusive greenish-blue; the color and amount of residual reflection depend on the angle of view