Properties of CONTURAN®

CONTURAN® is an anti-reflective glass with optical interference coatings between 50 nm and 100 nm thick applied to both sides by dip coating. In contrast to conventional, uncoated glass, CONTURAN® provides the best view at all times. Use this innovative special glass technology with crystal clear competitive benefits for your products.



Less reflection – high transmission
See for yourself, with your own eyes, the product benefits that CONTURAN® can offer you compared to standard float glass. Its reduced reflection and resultant high light transmission guarantees an unrestricted view.




Visual color impression
In transmission, the visual rating of CONTURAN® is color neutral. CONTURAN® Standard and Magic show a greenish tinge in the reflection. A blue-violet anti-reflective coating can, however, be supplied on request. The reflection from CONTURAN® Grey is blue-violet.




High chemical resistance
CONTURAN® has proved its chemical resistance in a range of test methods. Its anti-reflective coating has demonstrated that it is resistant to drinks and cockpit sprays. The Copper Accelerated Acetic Acid-Salt Spray Testing has confirmed its good resistance to corrosion: no peeling off of coating visable.


Further processing for greater safety
CONTURAN® can be used in the form of thermally toughened glass (for safety glass 4 mm thick) or as laminated safety glass CONTURAN® Protect. The optical properties of the latter are the same as for CONTURAN® Standard or alternatively CONTURAN® Magic of the same total thickness.