SCHOTT North America |
Radiation Shielding Glass
Optimal radiation protection
|
 |
RD 50™ radiation shielding glass
|
If radiation penetrates the human tissue, there is a risk of damage to tissue and organs. Radiation Shielding Glasses RD 50™ and RD 30 provide optimum protection, as they contain a high percentage of lead oxide, absorbing the rays.
The figure "50" stands for a min. 5,05 g/cm³ density.
The figure "30" stands for a min. 3,13 g/cm³ density.
Which glass is used depends on the lead equivalent, which is determined for each application.
|
Health protection
|
The Radiation Shielding Glasses RD 50™ and RD 30 provide the best protection for:
|
Technicians monitoring the x-ray process in medicine and industry
Technicians at mammography work stations
Technicians in research and development (i.e. "glove-box")
|
The type of Radiation Shielding Glass to use depends on the dose of radiation.
|
Small glass thickness
|
RD 50™ provides high radiation absorption with a small glass thickness
|
Shock resistant
|
RD 30 can be thermally toughened and supplied as safety glass (ESG)
|
Insulated glass
|
RD 50™ / RD 30 can be processed to insulated glass
|
Laminated glass
|
Both RD 50™ and RD 30 can be processed as laminated safety glass.
|
Short delivery time
|
Max. 3-4 weeks delivery time after order receipt
|
Glass versus Synthetic material(Acrylic)
|
- X-ray protection glass RD 50™ / RD 30 is much thiner and lighter than acrylic with equivilent lead protection.
Thickness and weight comparison for a lead equivalent of 2,2 mm Pb:
- RD 50™ thickness: 7,0-8,5 mm 43 kg/qm
in comparison to:
- Acrylic thickness: 44,0-48,0 mm 74 kg/qm
- RD 50™ / RD 30 are always edge processed. Acrylic is not
- RD 50™ / RD 30 are anti-static, therefore they do not soil so easily
- RD 50™ / RD 30 can be disinfected with UV-C
- RD 30 can be thermally tempered
- Insulated glass can be processed
- Laminated glass can be processed
- Synthetic material absorbs steam
- RD 50™ / RD 30
are:
- More resistant against available disinfectants
- More scratch resistant
- Nonflammable
|
|
|