N-FK58 XLD: Temperature coefficients of refraction now available

SCHOTT Advanced Optics offers an updated datasheet for the optical glass N-FK58 XLD, a high quality optical glass with extremely low Dispersion (XLD = extremely low dispersion) and excellent processing properties. The datasheet for N-FK58 XLD now also includes the temperature coefficients of refraction. This new data makes it possible to exactly determine the temperature dependence of the refractive index, allowing for minimal effects of temperature changes in the optical design and final performance of the application.

Contact
SCHOTT North America, Inc.
400 York Avenue
Duryea, PA 18642
USA
E-Mail to SCHOTT570-457-7485
News, Exhibitions & Events
15.
May
Exhibition Optatec, Frankfurt, Germany, 05-15 to 05-17-2018
25.
April
Exhibition OPIE - Space & Astronomical Optics EXPO, Yokohama, Japan, 04-25 to 04-27-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.