Down-Draw Process

Down-Draw Process of SCHOTT Advanced Optics
The down-draw process developed exclusively by SCHOTT is used in Grünenplan to produce thin glasses and ultra clear flat glasses. During this process, a ribbon of glass is pulled down from the top, moving across various drums and through the cooling track.

Advanced Optics uses this process to produce SCHOTT AS 87 eco, the D 263® series, and AF 32® eco glasses, among others.

Main characteristics of the down-draw process
  • A flawless surface with a surface roughness of < 1nm
  • Broad thickness spectrum from 1.1 to 30 µm
  • Fast conversion to various glass types
  • Very high TTV (total thickness variation) and curvature specifications
  • High flexibility in regards to output and thickness.
Contact
SCHOTT North America, Inc.
400 York Avenue
Duryea, PA 18642
USA
E-Mail to SCHOTT570-457-7485
News, Exhibitions & Events
14.
March
Exhibition LOPEC, Munich, Germany, 03-14 to 03-15-2018
06.
March
Exhibition IT Trans, Karlsruhe, Germany, 03-06 to 03-08-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.