High-Precision Dilatometer

Quality assessment of our ZERODUR® glass ceramic with extremely low thermal expansion coefficients ranging from 0 ± 1 · 10–7 · K-1 to 0 ± 7 · 10–9 · K-1 requires high-precision measurement equipment.

SCHOTT’s specially developed pushrod dilatometer combines state-of-the-art technology with our many years of experience. The pushrod dilatometer is capable of measuring coefficients of thermal expansion (CTE) in ZERODUR® with a reproducibility of up to 1 · 10–9 (1 ppb/K) as standard in a temperature range of 0 °C to 50 °C. On request, the thermal expansion coefficient can also be determined for an extended temperature range.
Contact
SCHOTT North America, Inc.
400 York Avenue
Duryea, PA 18642
USA
E-Mail to SCHOTT570-457-7485
News, Exhibitions & Events
14.
March
Exhibition LOPEC, Munich, Germany, 03-14 to 03-15-2018
06.
March
Exhibition IT Trans, Karlsruhe, Germany, 03-06 to 03-08-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.