Sapphire

Product Information



Sapphire, as one of the hardest, most durable and scratch resistant materials, offers a broad transmission range from UV to mid infrared wavelengths (250 – 5000 nm). The material is able to withstand extreme environmental conditions and temperature changes.

SCHOTT offers sapphire windows in different supply forms, dimensions, and in customized processing stages.



On this page the following categories are addressed:

Material
Advantages
Applications
Transmission Curve
Forms of Supply


Material

  • Extreme hardness & high mechanical strength (withstands extreme environmental conditions)
  • Excellent thermal conductivity/heat resistance
  • High transmittance (UV to IR)
  • Low dn/dT
  • High electrical resistance (1014 Ohm-cm)
  • High dielectric constant (9.39 from 1.0 MHz to 8.5 GHz)


Advantages

  • SCHOTT offers sapphire material in optical quality
  • Customized characteristics concerning dimensions and shapes (round, square, and more, diameters up to 300 mm)
  • Polished surface and customized coating for different applications
  • Best Practice in sapphire processing due to longterm experiences from handling optical materials
  • Usage of most advanced equipment and state-of-the-art metrology for manufacturing and quality control


Applications

  • Infrared applications (e.g. radiometry, optical guidance systems, gas analysis, medicine, safety and security)
  • High-pressure and shock-loading applications (e.g. chamber or heater windows in chemical process equipment)
  • Optical applications (e.g. optical components from UV to IR)
  • Scratchproof sapphire watch glasses


Transmission Curve




Forms of Supply


  • Customized processing: polishing and coatings (e. g. antireflective coating)
  • Plano and spherical surface
  • Various shapes from round to square


Attribute Commercial Quality Precision Quality Ultra precision quality
Size (round and square)
Ø from 10 to 300 mm
 from 10 to 210 mm
Size Tolerance1 ± 0,2 mm ± 0,10 mm ± 0,05 mm
Thickness1
From 1 to 40 mm
Thickness Tolerance1 ± 0,2 mm ± 0,10 mm ± 0,05 mm
Parallelism1 < 5 arc minutes < 1 arc minutes < 30 arc seconds
Surface Accuracy (PV)1 5 λ (546 nm) λ/2 (546 nm) λ/10 (546 nm)
Surface Quality
(scratch and dig)
According to MIL
80 - 50
According to MIL
40 - 20
According to MIL
20 - 10
Surface Roughness (Rq) < 10 nm < 3 nm < 1 nm
AR Coating
Custom designed
Order quantity
Upon customer specification. Please call sales representative.
Delivery Time (week)
6 - 10 weeks, upon raw material availability.


1 Upon geometry

Sapphire - Product Flyer
Contact

SCHOTT North America, Inc.

400 York Avenue
Duryea, 18642
USA
 570-457-7485
 570-457-7330
E-mail
Directions
More contacts
Trade Fairs & Events

06-18 to 06-21-2012

Nanotech Conference & Expo 2012

Santa Clara, CA

08-14 to 08-16-2012

SPIE Optics & Photonics

San Diego

10-16 to 10-17-2012

Frontiers in Optics

Rochester, NY

More trade fairs