SCHOTT Home
SCHOTT US Mexico USA
SCHOTT North America

Diffractive Optical Elements (DOEs)

Product Information



Diffractive Optical Elements (DOEs) are becoming key elements for laser optics, sensor optics and lighting applications. DOEs have the advantage to combine several optical functions needed for miniaturizing of optics. They are used to diffract and shape light into the area of interest.

Until now, diffractive optical elements for mass production could only be manufactured out of plastic, with all of its known weaknesses, including high scattering losses and low resistance to temperature, moisture, lasers and chemicals.

Now SCHOTT Advanced Optics has come up with a alternative made from glass. Glass components have the advantage of having lower dispersion than polymers and of being more thermally stable, as well as more mechanically and chemically resistant.

DOEs made from high index glass feature high diffraction efficiency of up to 95%. Not only do they exhibit high mechanical, thermal and chemical durability, it is also possible to combine various optical functions inside this single element.

How does it work?

Extremely small elements diffract light inside minute spaces, then bundle it into beams with exact shapes and direct it in the desired direction.

Benefits

SCHOTT Advanced Optics uses the precision molding technique to manufacture DOEs, pressing the contours of the highly precise shaping tool into the surfaces of glass thousands of times in an identical manner. No other company is capable of manufacturing these types of optics with such reproducible results.

Other benefits include:
  • High mechanical, thermal, and chemical durability
  • High diffraction efficiency of up to 95% due to the glass material instead of plastic
  • The ability to bend and direct light as desired in a minute space helps in the miniaturization of optical systems


Key Applications

DOEs are used in laser optics, optical sensors, and lighting applications.

Forms of Supply

SCHOTT Advanced Optics can provide DOEs according to customers’ specifications with a maximum size of 70 X 70 mm.

Specifications

Phase Levels
2
16
Period Size
> 1 µm
> 8 µm
Efficiency
up to 40 %
up to 95 %
Depth
< 10 µm
< 10 µm
Aspect Ratio
< 1:1
< 1:1
Side slope
< 80 °
< 80 °


Quality Assurance

Our quality control is based on self-checking during production and 100% final inspection. Measuring instruments include 2D profile measuring and holographic interferometer measuring.

Any Related Information

Diffractive Optical Elements - Product Flyer
Contact

SCHOTT North America, Inc.

400 York Avenue
Duryea, 18642
USA
 570-457-7485
 570-457-7330
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

04-24 to 04-26-2012

Defense, Security and Sensing 2012

Baltimore, MD

05-08 to 05-10-2012

CLEO

San Jose, CA

06-18 to 06-21-2012

Nanotech Conference & Expo 2012

Santa Clara, CA

More trade fairs