CNC machined parts are parts which have been processed to complex forms. These parts have a matte (non-transparent) finish, as they have been processed with diamond tools. The process involved typically uses 3- or 5- axis machines, coupled with the use of CAO software, nearly all-geometrical forms can be achieved.

Precision CNC Machined Parts Benefits



SCHOTT Advanced Optics has accumulated many years of experience in the production of precision CNC machined blanks and has a variety of CNC machines available.

In addition, we can:
  • Produce prototypes as well as ramp up to serial production
  • Supply precision blanks instead of raw glass, saving our customers the investment and administration efforts involved with raw glass stock
  • Reduce inner stress caused by diamond machining by chemical (acid etching) or thermal treatment (tempering).


Key Applications



Precision CNC machined blanks are often put to optical and mechanical uses in applications such as:
  • Photolithography
  • Avionics
  • Medical
  • Astronomy
  • Metrology


Precision CNC Machined Parts Materials



Precision CNC machining can be applied to all types of optical and color glass, as well as ceramics. Some commonly processed materials include:
  • Borosilicate glass
  • Filter glass
  • Optical glass
  • Technical glass
  • ZERODUR® glass ceramic


Precision CNC Machined Parts Forms of Supply



CNC machined parts can be supplied in dimensions up to 2550 x 700 x 500 mm or 1000 x 1000 x 1000 mm.

Precision CNC Machined Parts Specifications



We can produce machined blanks in line with our customers' specifications and ISO 10110 specifications.
  • General dimensional tolerances: up to 0.010 mm
  • Surface roughness: G3 (up to 0.4 µm Rq)
  • Flatness: 0.005 mm / 100 mm
  • Small holes up to 0.5 mm diameter


Quality Assurance



Our quality control is based on self-checking during production, random inspection, and a 100% final inspection. Equipment we use include: 3D optical measurement (Smart Scope), 3D measurement machines, profile projector as well as surface profiling (Talysurf). Complex forms are also measured with Form Talysurf. Inspection reports are available upon request.

Contact

SCHOTT North America, Inc.

400 York Avenue
Duryea, 18642
USA
 570-457-7485
 570-457-7330
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

04-24 to 04-26-2012

Defense, Security and Sensing 2012

Baltimore, MD

05-08 to 05-10-2012

CLEO

San Jose, CA

06-18 to 06-21-2012

Nanotech Conference & Expo 2012

Santa Clara, CA

More trade fairs