Optical Glass Coatings

Optical Glass Coatings Product Information



Optical Glass Coatings

SCHOTT Advanced Optics performs standard and custom-designed optical glass coatings. We deposit optical thin film coatings onto glass and other substrates for spectral wavelengths between 200 and 3000 nm.

Important optical glass coating types include:
  • Reduce reflection: Anti-reflective (AR) coating, spectral range in UV, VIS, IR
  • Increase reflection: mirror coating (metallic or dielectric)
  • Beam splitters
  • Polarizers
  • Neutral density filter coating
  • Laser coating with high resistance to flux
  • Demist coating RIA 2
  • Bandpass Coating
  • ITO coating
  • SIO2 protective coatings
”Hard coatings” do not need any additional protection, because the layers usually consist of very stable metal oxides. ”Soft coatings” usually require additional measures to protect the filters. This can be achieved by a supplementary cementing with a suitable glass.

Within certain areas of the UV spectrum it is not possible to use optical elements due to the inherent absorption involved. In such cases the coated substrates are fitted into appropriate mounts and protected by suitable glass.

Optical Glass Coatings Benefits



SCHOTT Advanced Optics is a trusted supplier of coated products due to our long experience and reliable process stability. With our expertise, we can provide:
  • Different types of optical glass coating on substrates of different sizes and materials
  • Different values for half width (HW)
  • Continuously alterable half widths (i-line filters, band passes)
  • Ion plating: specific temperature stability possible


Optical Glass Coatings Key Applications



Optical glass coatings are often required for substrates used in:
  • Optical systems
  • Laser systems
  • Illumination
  • Space applications
  • Defense applications
  • Medical applications
  • Industrial sectors.

Optical Glass Coatings Materials



All types of materials can be coated:
  • Borosilicate glass
  • Contrast enhancement glass types, etc.
  • Filter glass
  • Optical glass
  • ZERODUR® glass ceramic


Forms of Supply



Our standard forms of coated substrates range from 1 mm to 400 mm. Larger dimensions, such as 900 x 900 mm, AR and Aluminum mirror plates are also available.

Optical Glass Coatings Specifications



We can coat substrates with diameters between 1 mm and 400 mm. The spectral range is between 200 and 3000 nm. Since a very broad range of specifications can be met, please use the bandpass-, longpass-or shortpass-filter questionnaire in the interference filter catalog.

Ion Plating (IP)
  • Plasma Assisted Deposition with the Leybold-Advanced Plasma Source (APS)
  • Cold electron beam evaporation


Quality Assurance



We measure the quality of our optical glass coating with a spectrophotometer (measurement between 200 nm and 3000 nm), and also conduct direct or indirect monochromatic monitoring with quartz crystal and optical thickness measurements.

We can also deliver test glasses upon request.

Related Information



You could be interested in our low Tg optical glasses for precision molding.

Coating (Product Flyer)Scratch resistant AR Coating (Product Flyer)
Contact

SCHOTT North America, Inc.

400 York Avenue
Duryea, 18642
USA
 570-457-7485
 570-457-7330
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

04-24 to 04-26-2012

Defense, Security and Sensing 2012

Baltimore, MD

05-08 to 05-10-2012

CLEO

San Jose, CA

06-18 to 06-21-2012

Nanotech Conference & Expo 2012

Santa Clara, CA

More trade fairs