Anti-reflection coating in accordance with ISO 9211.
Our broad band AR coatings can be applied to a wide range of different glasses in order to minimize the Fresnel reflections of the substrate.
This coating can be optimized for your requirements in the range of 350 nm to 1000 nm.


Features

  • The maximum diameter of the substrate is  350 nm.
  • The coating is washable and scratch resistant.
  • The operating temperature is up to 250 °C for several hours.
  • Reflection r over a large range of wavelengths.

Additional functions

On special request we can add the following functions to the AR coating:
  • Abrasion resistance
  • Humidity resistance
  • Resistance against acids or alkalines
  • Easy cleaning

Detailed specifications on request.
 
Contact
SCHOTT North America, Inc.
400 York Avenue
Duryea, PA 18642
USA
E-Mail to SCHOTT570-457-7485
News, Exhibitions & Events
14.
March
Exhibition LOPEC, Munich, Germany, 03-14 to 03-15-2018
06.
March
Exhibition IT Trans, Karlsruhe, Germany, 03-06 to 03-08-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.