Prisms are available as:

Supply Forms
Dimensions
Examples of Products
Pressings 10 – 200 mm
  • Right-angle prisms
  • Rhomboid prisms
  • Penta prisms
  • TIR prisms
  • Cube beamsplitters
  • Roof prisms
  • Porro prisms
Cut blanks
Prisms
  • polished
Prisms
  • coated
Sub-assemblies
Depending on the customer’s specifications, two different manufacturing processes are possible at SCHOTT to offer the best possible quality and manufacture to more efficiently:

1) Pressing:

Melting → Pressing → Polishing → Coating → Sub-assembly

2) CNC machining:

Melting → CNC-sawing (cut blank) → Polishing → Coating → Sub-assembly