SCHOTT PYRAN®

Summary

ISO PYRAN® S – At a glance

Technical data

Product Fire Rating Thickness Ug-Value g-Value Light Transmission Sound Reduction
  acc. EN 13501
[mm]
[W/m2K]
[%]
[%]
[dB]
Double glazing units
ISO PYRAN® S E(G) 30
24
2.7
78
83
33
E(G) 30
26
2.7
75
82
34
E(G) 30 - 90
25
2.7
78
83
33
E(G) 30 - 90
27
2.7
75
82
33
Heat insulation - Low e coatings
ISO PYRAN® S E(G) 30
24
1.4
61
82
33
E(G) 30
24
1.4
65
82
33
E(G) 30 - 90
25
1.4
61
82
34
E(G) 30 - 90
25
1.4
65
82
34
ISO PYRAN® S-D E(G) 30 - 60
28
1.4
55
79
 
E(G) 30 - 60
28
1.4
64
79
 
E(G) 30 - 60
30
1.4
54
78
39
E(G) 30 - 60
30
1.4
64
78
39
Sun protection - Solar control coatings
ISO PYRAN® S E(G) 30
26
1.5
27
50
34
E(G) 30
26
1.5
22
41
34
E(G) 30
26
1.5
17
30
34
E(G) 30
26
1.5
30
47
34
E(G) 30 - 90
26
1.5
27
50
33
E(G) 30 - 90
26
1.5
22
41
33
E(G) 30 - 90
26
1.5
17
30
33
E(G) 30 - 90
26
1.5
30
47
33
Sound insulation
ISO PYRAN® S-D E(G) 30 - 60
35
2.7    
42
E(G) 30 - 60
30
1.4 54 78
39
E(G) 30 - 60
30
2.7    
41
E(G) 30 - 60
45
2.7
   
43
E(G) 30 - 60
45
2.7
   
43
E(G) 30 - 60
34
2.7    
45

Contact

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976

At a glance

Areas of application

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

ISO PYRAN® S – Technical data

TECHNICAL INFORMATION
Product Fire Rating Thickness Ug-Value g-Value Light Transmission Sound Reduction
  acc. EN 13501
[mm]
[W/m2K]
[%]
[%]
[dB]
Double glazing units
ISO PYRAN® S E(G) 30
24
2.7
78
83
33
E(G) 30
26
2.7
75
82
34
E(G) 30 - 90
25
2.7
78
83
33
E(G) 30 - 90
27
2.7
75
82
33
Heat insulation - Low e coatings
ISO PYRAN® S E(G) 30
24
1.4
61
82
33
E(G) 30
24
1.4
65
82
33
E(G) 30 - 90
25
1.4
61
82
34
E(G) 30 - 90
25
1.4
65
82
34
ISO PYRAN® S-D E(G) 30 - 60
28
1.4
55
79
 
E(G) 30 - 60
28
1.4
64
79
 
E(G) 30 - 60
30
1.4
54
78
39
E(G) 30 - 60
30
1.4
64
78
39
Sun protection - Solar control coatings
ISO PYRAN® S E(G) 30
26
1.5
27
50
34
E(G) 30
26
1.5
22
41
34
E(G) 30
26
1.5
17
30
34
E(G) 30
26
1.5
30
47
34
E(G) 30 - 90
26
1.5
27
50
33
E(G) 30 - 90
26
1.5
22
41
33
E(G) 30 - 90
26
1.5
17
30
33
E(G) 30 - 90
26
1.5
30
47
33
Sound insulation
ISO PYRAN® S-D E(G) 30 - 60
35
2.7    
42
E(G) 30 - 60
30
1.4 54 78
39
E(G) 30 - 60
30
2.7    
41
E(G) 30 - 60
45
2.7
   
43
E(G) 30 - 60
45
2.7
   
43
E(G) 30 - 60
34
2.7    
45