ISO PYRANOVA®  

At a glance

ISO PYRANOVA® incorporates PYRANOVA® as part of a double-glazed unit that can be used wherever further requirements are needed in addition to protection from fire. In combination with other performance glasses, ISO PYRANOVA® fulfils functional, aesthetic and energy efficiency requirements.
  • Sun protection - Solar control coatings (anti-glare)
  • Heat insulation - Low e coatings
  • Sound insulation

Technical data

Product Fire Rating Thickness Ug-Value g-Value Light
Transmission
Sound Reduction
  acc. EN 13501-2
[mm]
[W/m2K]
[%]
[%]
[dB]
Heat insulation - Low e coatings
ISO PYRANOVA® for interior application EI (F) 30
34
1.4
54
74
40
EI (F) 30
34
1.1
54
74
40
ISO PYRANOVA® for exterior application EI (F) 30
38
1.4
54
73
40
EI (F) 30
38
1.1
54
73
40
ISO PYRANOVA® for interior application EI (F) 30
30
     
43
EI (F) 30
37
1.4
   
45
Sound insulation
ISO PYRANOVA® for exterior application EI (F) 30
42
1.4
   
46
EI (F) 30
44
1.4
   
47
EI (F) 30
44
1.4
   
45
EI (F) 30
54
     
47
EI (F) 30
52
     
49