NOVOLAY® secure is manufactured in a microfloat process with cutting-edge technology. A special float glass from SCHOTT with outstanding properties provides the basis for a wide variety of safety applications. In addition to its excellent homogeneity, it displays impressive optical quality – even surpassing white glass - while remaining low in specific weight. NOVOLAY® secure is suitable for impact and manual attack resistant glazing in accordance with EN 356 and bullet resistance in accordance with EN 1063.

Technical data

Glastype Article number EN 356 EN 1063 Fire resistance class Thick-
ness in mm
Weight in kg/m2

Manual attack resistance - Standard products
NOVOLAY® secure P4A 2.4.2 P4A - E 60 10 23
NOVOLAY® secure P5A 3.13.10 P5A - - 11 23
NOVOLAY® secure P6B 2.2.2 P6B - - 15 27
NOVOLAY® secure P7B 2.9.3 P7B - - 18 33
NOVOLAY® secure P8B 1.9.3 P8B - - 18 32

Manual attack resistance -
Special products (suitable for panic doors RC 2 – RC 4)
NOVOLAY® secure P8B P2 1.5.10 P8B P2 - - 20 35
NOVOLAY® secure P8B PRC3 7.11.52) P8B PRC3 - - 34 58
NOVOLAY® secure P8B PRC4 7.12.0 P8B PRC4 - - 50 82

Bullet resistance - Standard products
NOVOLAY® secure BR2NS 1.2.3   BR2NS - 17 32
NOVOLAY® secure BR2NS 1.4.5   BR2NS
EW 30/
E 60
24 52
NOVOLAY® secure BR4NS 15.3.0   BR4NS - 20 41
NOVOLAY® secure BR4NS 1.5.4 P8B BR4NS - 44 96
NOVOLAY® secure BR6NS 1.3.3 P8B BR6NS - 40 80
NOVOLAY® secure BR6NS 1.5.7 P8B BR6NS EI 30 /
EW 60
63 137
NOVOLAY® secure BR7NS 1.1.2 P8B PRC3 BR7NS EI 45 /
EW 60
74 162
ISO NOVOLAY® secure BR4NS 1.6.5   BR4NS - 50 93
ISO NOVOLAY® secure BR4NS 1.6.6   BR4NS - 60 94

Fire protection & Bullet resistance - Standard products
NOVOLAY® secure BR6NS 1.5.7 P8B BR6NS EI 30 /
EW 60
63 137
NOVOLAY® secure BR7NS 1.1.2 P8B BR7NS EI 45 /
EW 60
74 162
1) suitable for panic doors WK 3
2) suitable for panicsdoors RC 3

Downloads

Exhibitions & Events
27.
June
Exhibition Sicherheitsexpo, München, Germany, 06-27 to 06-28-2018
14.
January
Exhibition BAU, Munich, Germany, 01-14 to 01-19-2019
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.