BMW Welt, München
BMW Welt, München

PYRAN® S-P

At a glance

Key facts

PYRAN® S-P

Systems that use PYRAN® S-P require no frame constructions whatsoever. This is the result of a perfect symbiosis between glass panes connected to each other by joints that are barely noticeable and point mounts and brackets that secure the glass panes to a strong, yet light, supporting structure. The panes remain permanently fixed in place, free of tension and without slippage under even the most extreme conditions, such as heavy loads created by wind pressure or suction.


  • Borosilicat-SG
  • Classification:
    E 30

Technical data

Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34

Contact

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

PYRAN® S-P

Systems that use PYRAN® S-P require no frame constructions whatsoever. This is the result of a perfect symbiosis between glass panes connected to each other by joints that are barely noticeable and point mounts and brackets that secure the glass panes to a strong, yet light, supporting structure. The panes remain permanently fixed in place, free of tension and without slippage under even the most extreme conditions, such as heavy loads created by wind pressure or suction.


  • Borosilicat-SG
  • Classification:
    E 30
Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34