PYRANOVA® for exterior applications 

At a glance

PYRANOVA® for exterior applications is a special glass for use in external or particulary difficult situations, a clear composite safety glass for fire resistant glazing that offers fire resistant properties in accordance with DIN EN ISO 12543.

Depending on its structure, it is manufactured from at least two float glass panes with transparent, fire resistant intumescent interlayers and an external pane made of laminated safety glass. [Edit Content]

Technical data

Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
  acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Exterior
PYRANOVA® EW EI 15 / EW 30
10
24
87
5.4
36
PYRANOVA® EW EI 15 / EW 30
14
32
86
5.2
38
PYRANOVA® 30 EI 30
19
44
83
5
38
PYRANOVA® 45 EI 45 / EW 60
19
44
85
5
38
PYRANOVA® 60 EI 60
27
61
86
4.7
41
PYRANOVA® 90 EI 90
40
93
83
4.1
44
PYRANOVA® 120 EI 120
54
116
74
2.5
44