SCHOTT PYRAN®

Summary

PYRAN® G – At a glance

Technical data

Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
 
  acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® G E 30
6
13.7
 
91
92
31
E 30
8
18.2
 
90
92
32

Contact

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976

At a glance

Areas of application

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

Product types

PYRAN® G – Technical data

TECHNICAL INFORMATION
Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
 
  acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® G E 30
6
13.7
 
91
92
31
E 30
8
18.2
 
90
92
32

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976