SCHOTT PYRAN® S-SF

At a glance

Technical data

Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[k/Wm2]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34

Contact

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet
Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[k/Wm2]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976