Technical data

Product Fire Rating Thickness Weight Ug-Value g-Value Light Transmission Sound Reduction
  nach EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 120
6
13.7
 
91
92
31
E(G) 30 - 120
8
18.2
 
90
92
32
E(G) 30 - 120
10
22.8
 
90
92
33
E(G) 30 - 120
12
27.4
 
90
92
34
*PYRAN® butt jointed glazing is available for fire rating E 30 and E 60

Contact

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976

At a glance

Areas of application

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

Product types

PYRAN® S – Technical data

TECHNICAL INFORMATION
Product Fire Rating Thickness Weight Ug-Value g-Value Light Transmission Sound Reduction
  nach EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 120
6
13.7
 
91
92
31
E(G) 30 - 120
8
18.2
 
90
92
32
E(G) 30 - 120
10
22.8
 
90
92
33
E(G) 30 - 120
12
27.4
 
90
92
34
*PYRAN® butt jointed glazing is available for fire rating E 30 and E 60

Daniel Poling

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA

 +1 (502) 657-4423
 +1 (502) 966-4976