The resistance of BOROFLOAT® 33 to thermal and mechanical loads is improved by thermal semi-toughening.

Thermal semi-toughening is possible in thicknesses from 3.3 to 15 mm. The maximum sheet size is 3,000 x 1,800 mm and the minimum edge length is 300 mm. We will be happy to provide information about thicknesses and sizes at any time upon request.