Thicknesses and Sizes



BOROFLOAT® 33 can be cut to smaller sizes as required by customers.
A wide thickness range from 0.7 to 25.4 mm is available.

Standard Sizes Thicknesses Packing
1150 x 850 mm   0.7 - 25.4 Small wooden case or Triwall
1700 x 1300 mm 16.0 - 21.0 mm Large wooden case
2300 x 1700 mm   3.3 - 15.0 mm Large wooden case


Max. dimensions for stock sizes: 3000 x 2300 mm (Dicken 5.5 - 9.0 mm)
Minimum dimensions for stock sizes: 700 x 575 mm



We will be happy to provide information about other sizes upon request.


The quality of BOROFLOAT® 33 is ensured by a proven quality management system in compliance with the requirements of DIN ISO 9001.