Thickness range

BOROFLOAT® 33 is offered in the following
thicknesses and tolerances, in mm:


Thickness in mm ( inch )
Tolerance in mm ( inch )
0.70  (0.027)
±0.07  (0.003)
1.10  (0.043)
± 0.1  (0.004)
1.75  (0.069)
± 0.1  (0.004)
2.00  (0.079)
± 0.2  (0.008)
2.25  (0.089)
± 0.2  (0.008)
2.75  (0.108)
± 0,2  (0.008)
3,30  (0.130)
± 0,2  (0.008)
3,80  (0.150)
± 0,2  (0.008)
5,00  (0.197)
± 0,2  (0.008)
5,50  (0.216)
± 0,2  (0.008)
6,50  (0.256)
± 0,2  (0.008)
7,50  (0.295)
± 0,3  (0.012)
8,00  (0.315)
± 0,3  (0.012)
9,00  (0.354)
± 0,3  (0.012)
11,00  (0.433)
± 0,3  (0.012)
13,00  (0.512)
± 0,5  (0.020)
15,00  (0.590)
± 0,5  (0.020)
16,00  (0.630)
± 0,5  (0.020)
17,00  (0.670)
± 0,5  (0.020)
18,00  (0.708)
± 0,5  (0.020)
19,00  (0.748)
± 0,5  (0.020)
20,00  (0.787)
±0,7  (0.027)
21,00  (0.827)
± 0,7  (0.027)
25,40  (1.000)
± 1,0  (0.040)