05-29-2014, SOUTHBRIDGE, Mass. and SANTA FE, N.M.

SCHOTT POWERAMIC™ Glass-Ceramics: A New Class of Dielectrics for High Voltage Capacitors

Glass-ceramics as dielectrics in capacitors provide high energy storage density for an extended temperature range
The international technology group SCHOTT has developed a new dielectric material. POWERAMIC™ is a family of highly homogenous, pore-free glass-ceramics. Providing very high energy storage density, these materials show excellent dielectric properties even at elevated temperatures. In high voltage applications this allows for smaller, lighter weight passive components such as capacitors to deliver a more powerful performance. SCHOTT will introduce this innovation at IEEEs 2014 International Power Modulator and High Voltage Conference (IPMHVC) in Santa Fe, New Mexico from June 1 to 4 at Booth 26.
POWERAMIC™: This new class of glass-ceramic materials introduced by SCHOTT offers extraordinarily high energy storage density in combination with excellent temperature characteristics for smaller and lighter weight high voltage capacitors. Source: SCHOTT.
POWERAMIC™: This new class of glass-ceramic materials introduced by SCHOTT offers extraordinarily high energy storage density in combination with excellent temperature characteristics for smaller and lighter weight high voltage capacitors. Source: SCHOTT.

Capacitors are passive electrical components that store energy in the form of an electrostatic field in the dielectric material between metal contacts. They are commonly used to buffer, stabilize or couple the voltage and power flow in electric power conversion systems. High voltage capacitors are becoming increasingly required; for example in Excimer Lasers for industrial and medical applications, for medical x-ray equipment, for high voltage power supplies (HVPS) for industrial applications, and for grids for renewable energy.

Higher voltages and current densities, however, lead to an increasing thermal load. Current capacitor technologies for high power applications are mostly based on polypropylene (PP) or N4700 ceramic. Both are limited to temperatures below 90° C due to either their loss of capacitance (N4700) or their loss of reliability (PP) with rising temperatures. SCHOTT’s new class of POWERAMIC™ materials shows a superior performance regarding energy storage density and dielectric properties in an expanded temperature range.

POWERAMIC™ glass-ceramics are highly homogenous and pore free which supports their high dielectric breakdown strength and leads to storage density exceeding that of current capacitor solutions by a factor of up to ten. It allows the construction of smaller and lighter weight capacitors,” says Dr. Martin Letz, Senior Principal Scientist at SCHOTT Research & Technology Development. “The nano-sized crystalline structure of POWERAMICTM glass-ceramics, which is tightly controlled in a truly amorphous glassy phase, improves the dielectric properties at higher field strength and expands the temperature range compared to ceramic capacitors,” he adds.

SCHOTT has more than 40 years of experience in developing and producing glass-ceramics and is a world leading supplier for a number of products such as ZERODUR® glass-ceramic with a virtually zero thermal expansion used for mirror substrates in astronomic telescopes, CERAN® glass-ceramic cooktop panels, ROBAX® glass-ceramic viewing panels for fireplaces and NEXTREMA® glass-ceramic for extreme industrial applications. By applying the same production method to a different chemical composition, SCHOTT created a new class of high performance dielectrics. POWERAMIC™ glass-ceramics are titanate-based. As glass-ceramics, they are produced in a two-step process: at first, a transparent glass with a totally amorphous structure is melted and hot-formed as a solid, amorphous glass. In the second step, a well-defined time-temperature profile is applied to grow nano-sized crystals within the glass. Their unique properties are achieved by using highly specified and controlled chemical compositions and processes that allow for narrow tolerances and a reliable stable quality.

POWERAMIC™ glass-ceramic is supplied as a qualified semi-finished product for the production of capacitors, upon request also in metallized form. It can be used for all commercially available capacitor designs, e.g. doorknob/hockey puck capacitors, SLCs (single layer capacitors), SMD (surface mount device) capacitors, as well as in custom designs to individual customer specifications.

For additional information visit:

Download link for the photo accompanying this release:

More press pictures can be downloaded at:

SCHOTT is an international technology group with more than 130 years of experience in the areas of specialty glass and materials and advanced technologies. SCHOTT ranks number one in the world with many of its products. Its core markets are the household appliance, pharmaceutical, electronics, optics and transportation industries. The company is strongly committed to contributing to its customers’ success and making SCHOTT an important part of people’s lives with high-quality products and intelligent solutions. SCHOTT is committed to managing its business in a sustainable manner and supporting its employees, society and the environment. The SCHOTT Group maintains close proximity to its customers with manufacturing and sales units in 35 countries. Its workforce of 15,400 employees generated worldwide sales of $2.5 billion for the 2012/2013 fiscal year.

Press contacts:

Barbara Augenblick

SCHOTT North America, Inc.
Phone: 914-831-2285
Fax: 914-831-2201

Mike Lizun
Gregory FCA on behalf of SCHOTT
Office: 610-642-1435

Further information
SCHOTT North America, Inc.
Barbara Augenblick
555 Taxter Road
Elmsford, NY 10523
Phone: 914-831-2285
Exhibitions & Events
Exhibition PDA Annual Meeting, Orlando, FL, USA, 03-19 to 03-21-2018
Exhibition Pre-filled Syringes East Coast, Boston, MA, USA, 04-11 to 04-12-2018
Exhibition SPIE Defense + Commercial Sensing, Orlando, FL, USA, 04-17 to 04-19-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.