SF-K Data

Dimensions

Dimension (Unit:mm)

Ratings

Part
Number
Rated
Functioning
Temperature
Tf
(℃)
Operating
Temperature
(℃)
2)
Th
(℃)
Tm
(℃)
Rated
current3)
Rated
Voltage
SF70K 73 70±2 45



150




6A
(Resistive)
 





AC250V
SF76K 77 76±0/-4 51
SF90K 94 90±2 66
SF94K 99 94±2 84
SF96K 99 96±2 71
SF119K 121 119±2 94
SF188K 192 188+3/-1 164
300
SF214K 216 214+1/-3 198
1) No use of hazardous substances prescribed by WEEE and RoHS.
All products do not use SVHC prescribed by REACH (174 substances, 7 July 2017).

2) Th is the maximum temperature measured on the thermal links when it continues to conduct a rated current without changing its state of conductivity for 168 hours, based on the standard of UL certification.

3) The following electrical ratings were used for the UL, VDE, and KTL safety standards: 10A (Resistive)/AC 250V.

Safety Standards

Part Number UL/cUL VDE BEAB CCC KTL PSE
Thailand Thailand Thailand Thailand Thailand
(SU05020
-*****)
Thailand
(JET1974-32001
-****)
SF70K
E71747
677802
-1171
-0006

C1180

1)

5004

1003
SF76K
SF90K
2)

-

2)

2)

1002
SF94K 2)
SF96K
E71747

677802
-1171
-0006

C1180


1)
5004
SF119K 5006 1004
SF188K
3) E71747
5007 1007
SF214K - 5008 1008
1) 2008010205282881
2) Pending approval.
3) The following SF-types have passed the Conductive Heat Aging Test (CHAT) specified by the UL safety standard: SF188K and SF214K.
Exhibitions & Events
30.
May
Exhibition Materials, Veldhoven, Netherlands, 05-30 to 05-31-2018
26.
June
Exhibition World Nuclear Exhibition, Paris, France, 06-26 to 04-28-2018
05.
September
Exhibition CIOE - China International Optoelectronic Expo, Shenzhen, China, 09-05 to 09-08-2018
17.
September
Exhibition Gastech, Barcelona, Spain, 09-17 to 09-20-2018
Contact
Electronic Packaging
SCHOTT North America, Inc.

15 Wells Street
Southbridge, MA 01550
USA
E-Mail to SCHOTT+1 (508) 765-7450
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.