SF-R Data

Dimensions

Dimension (Unit:mm)

Ratings

Part
Number

*:0/1
0:Standard
1:long
Rated
Functioning
Temperature
Tf
(℃)
Operating
Temperature
(℃)
2)
Th
(℃)
Tm
(℃)
Rated
current3)
Rated
Voltage
SF70R* 73 70±2 58




165












4)
15A/10A
(Resistive)












4)
AC250V
SF76R* 77 76+0/-4 62
SF81R* 84 81+3/-1 69
SF90R* 94 90±2 79
SF94R* 99 94±2 84
SF113R* 113 108±2 98
SF119R* 121 119±2 106
SF129R* 133 129±2 118
175
SF139R* 142 139±2 127
SF144R* 144 142±2 129
210
SF150R* 152 150+1/-3 137
SF167R* 167 164±2 153
250
SF184R* 184 182±2 174
SF188R* 192 188+3/-1 177
375
SF214R* 216 214+1/-3
200
SF229R* 229 227±2
380
SF240R* 240 237±2
Note 1) No use of hazardous substances prescribed by WEEE and RoHS.
All products do not use SVHC prescribed by REACH (174 substances, 7 July 2017).

2) For standard lead length type, add the suffix "0" at the end of the part number. For long lead length type, add the suffix "1" at the end of the part number.

3) Th is the maximum temperature measured on the thermal links when it continues to conduct a rated current without changing its state of conductivity for 168 hours, based on the standard of UL certification.

4) The electrical ratings according to the various safety standards are shown in the following table.
Rated Voltage UL/cUL VDE CCC KTL PSE5)
AC120V 20A (Resistive) - - - -

AC250V
10A (Resistive) 10A 10A 10A 10A
15A (Resistive) 15A 15A 15A 15A
16A (Resistive) - - - -

5) With respect to the PSE standard, SF-R is separately available for 10A and 15A ratings. Please select the appropriate product rating according to the specifications of the final application.

Safety Standards

1)Part Number
*:0/1
0:Standard
1:long
UL/cUL VDE CCC KTL 2)PSE
Thailand Thailand Thailand Thailand
(SU05020
-****)
Thailand
(JET1974-32001-****)
Rating 15A Rating 10A
SF70R*








E71747











677802
-1171
-0015












20130102
05600209



5004
2001 1003
SF76R*
SF81R*

2002


1002
SF90R*
SF94R*
SF113R* 5005 2003 1001
SF119R*


5006

2004

1004
SF129R*
SF139R*

2005


1005
SF144R*
SF150R*
SF167R*

5007
2006 1006
SF184R*


3)
E71747

2007

1007
SF188R*
SF214R*
5008
2008 1008
SF229R*
2009

1009
SF240R*
1) For standard lead length type, add the suffix "0" at the end of the part number. For long lead length type, add the suffix "1" at the end of the part number.

2)With respect to the PSE standard, SF-R is separately available for 10A and 15A ratings. Please select the appropriate product rating according to the specifications of the final application.

3) The following SF-types have passed the Conductive Heat Aging Test (CHAT) specified by the UL safety standard: SF184R*, SF188R*, SF214R*, SF229R*, and SF240R*.
Exhibitions & Events
30.
May
Exhibition Materials, Veldhoven, Netherlands, 05-30 to 05-31-2018
26.
June
Exhibition World Nuclear Exhibition, Paris, France, 06-26 to 04-28-2018
05.
September
Exhibition CIOE - China International Optoelectronic Expo, Shenzhen, China, 09-05 to 09-08-2018
17.
September
Exhibition Gastech, Barcelona, Spain, 09-17 to 09-20-2018
Contact
Electronic Packaging
SCHOTT North America, Inc.

15 Wells Street
Southbridge, MA 01550
USA
E-Mail to SCHOTT+1 (508) 765-7450
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.