Production Process

cutting
Cutting:
  • Automated straight cutting in 2 axes (x and y)
  • Shape cutting by CNC program
  • Water jet cutting
grinding
Grinding:
  • Double edge grinding
    (e.g. dubbed corners)
  • Shape grinding
    (e.g. complex shapes)
drilling
Drilling:

  • Typical diameter: 3.5 - 300mm
  • Various hole configurations and forms
  • Semi & fully automated processes
printing
Printing:
  • Hugh variety of color compositions
  • Each print requires an extra screen and printing process
  • Minimum line thickness: 0.3 mm
  • Minimum spot diameter: 0.5 mm
  • Thickness of a single print layer:
    10-20 µm
tempering & bending
Source: Markus Nikot
Tempering and Bending:
  • All products are thermally toughened using SCHOTT tempering techniques
  • Ceramic colors are fixed during this process
  • Bending is also available
Contact
SCHOTT Gemtron, Sweetwater TN
615 Highway 68
Sweetwater, TN 37874
USA
E-Mail to SCHOTT+1 (0) 423 337 3522
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.