RESISTAN® is a material family composed of various types of ceramics. Any material is not only distinguished by its outstanding thermal, chemical and optical properties, but also characterized by individual key features as well as optical appearances. The given examples are just a few application fields that RESISTAN® can be used in.

Clear transparent ceramics (e.g. RESISTAN® 724-3)

The transparent ceramics offer you all the advantages of a true temperature miracle with a clear view. In addition, it is highly permeable to thermal radiation, especially in the shortwave infrared range. As a result, clear transparent ceramics can be exemplary used for applications requiring very high thermal strength in combination with good transparency. [more]

Body-tinted ceramics (e.g. RESISTAN® 701-3)

The black body-tinted transparent ceramics outstand because of their excellent temperature durability in combination with high mechanical stability. Heat is transmitted very efficiently, with virtually no heat loss because of an almost exact heat permeability and a low thermal conductivity. The transmission of wavelength is optimized for the infrared range. [more]

Translucent ceramics (e.g. RESISTAN® 701-6)

Due to its low alkali content, translucent RESISTAN® has very unique insulating qualities. It is the ideal material for applications requiring an excellent insulator at high temperatures. In addition, this material meets highest standards on resisting chemical surface attacks. [more]

Opaque ceramics (e.g. RESISTAN® 724-8)

The opaque RESISTAN® is distinguished by its excellent resistance to chemical surface attacks by acid, alkali or hydrolytic effects. In addition, opaque RESISTAN® exceeds due to its absolutely dense and pore-free surface, which is also dirt-repellent and well-suited for clean room conditions. Furthermore, this material can be used for applications requiring good insulating properties. Aesthetics play an important role for non-transparent ceramics as well. The white appearance gives the material a noble and brilliant touch. [more]

We will be glad to provide further materials upon request.
For any other application, please send us your enquiry.

Contact

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA
 +1 (502)657-4417
 +1 (502)966-4976
E-mail
More contacts
Trade Fairs & Events