Due to its low alkali content, RESISTAN® has very outstanding insulating properties. It is the ideal material for applications requiring an excellent insulator at high temperatures.
Electrical properties of Resistan


Electrical Data
Specific Electrical Volume Resistance log ρ (250°C) [Ω·cm] 6.6 - 7.0
Specific Electrical Volume Resistance log ρ (350°C) 5.2 - 5.6
tk100 [°C] 173 - 198
Dielectric Constant εr (1 MHz, 25°C) 6.3 - 7.8
Dielectric Loss Tangent tan δ (1 MHz, 25°C) 0.004 - 0.02


Please find additional information and definitions in our glossary.

All technical data are intended to serve as typical averages and are subject to change.
Detailed information on the different material types are documented in separate data sheets [more] or can be provided upon request. [more]

Contact

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA
 +1 (502)657-4417
 +1 (502)966-4976
E-mail
More contacts
Trade Fairs & Events