Innovations

ROBAX® Dome

ROBAX® Dome is a round panel for stoves and fireplaces in form of a spherical segment.



Source: Spartherm Feuerungstechnik GmbH

Standard dimensions Mod. 1 Mod. 2
diameter
radius
height of dome
thickness
600.0 mm
500.0 mm
103.2 mm
4.0 mm
503.0 mm
340.0 mm
113.9 mm
4.0 mm
Mod. 3 Mod. 4
diameter
radius
height of dome
thickness

Other dimensions on request
400.0 mm
260.0 mm
96.4 mm
4.0 mm
311.0 mm
216.7 mm
68.6 mm
4.0 mm


ROBAX® Cone

ROBAX® Cone is a round bent panel in the form of a cone segment (can also be delivered with frame decoration). For more information regarding possible dimensions, please contact us.



Source: HWAM Heat Design AS

ROBAX® Giant

ROBAX® Giant is the biggest round bent vision panel for fireplaces in the world.
This panel can also be obtained with bevelled edges (Link) and/or drillings.

Dimensions
Bow length
Panel height
Thickness
1.490 mm
980 mm
4 and 5 mm




Source: Spartherm Feuerungstechnik GmbH

Contact

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA
 +1 (502)657-4418
 +1 (502)966-4976
E-mail
Directions
More contacts
Trade Fairs & Events

06-03 to 06-08-2012

Society for Information Display

Boston, MA

09-11 to 09-14-2012

Construct 2012

Phoenix, AZ

11-14 to 11-16-2012

GreenBuild

San Francisco, CA

More trade fairs