LABORATORY GLASS BOTTLES AND ACCESSORIES
DURAN® premium bottle with DIN thread, GL 45
- TÜV tested thermal shock resistance of 160 K, confirmed by GS-marking
- USP/neutral glass/FDA conformity for the entire system comprised of bottle, screw cap and pouring ring.
- Complete with premium screw cap with its PTFE coated silicone seal (colorless and temperature resistant from –196 °C to +260 °C)
|
 |
|
|
|
|
|
|
|
|
 |
 |
|
For more information about DURAN® Premium bottles click on the link below to download the catalog.
|
|
For more information on DURAN® laboratory glass bottles and accessories please refer to our catalog by clicking on the download link below:
|
|