This is how DURAN® is made

< 3 of 6 >



Manufacture
A wide range of precision manufacturing processes is used to produce DURAN® glass, three of which are described here: Drawing DURAN® glass tubing for technical applications in the chemical industry (A). Blowing glass hollow ware items on automated machines or, in the cases of special shapes or relatively small quantities, by glass makers (B). And pressing glass items such as desiccator bases on automated machines (C).