Capillary Arrays - High Density Hollow Fiber Arrays


SCHOTT’s High Density Capillary Arrays are manufactured for high performance defense applications such as radiation and bio-terrorism detection.

The glass processing technology developed by SCHOTT for these components is based on over 20 years of experience in the manufacturing of high resolution imaging components for military night vision, x-ray, industrial and scientific imaging applications.

SCHOTT uses this same advanced glass drawing technology to produce high precision, hollow glass Capillary Arrays in linear and plate formats in a variety of pore sizes and lengths.




Capillary Arrays can be custom manufactured In a wide variety of plate and linear formats.

All items herein are controlled by International Traffic In Arms Regulations (ITAR) or Export Administration Regulations (EAR).

High Density Hollow Fiber Arrays
Contact

Lighting and Imaging
SCHOTT North America Inc.

122 Charlton Street
Southbridge, MA 01550
USA
 +1 (508)765-9744
 +1 (508)764-6273
E-mail
Directions
More contacts
Trade Fairs & Events

04-25 to 04-26-2012

BIOMEDevice Show

Boston, MA

04-24 to 04-26-2012

Defense, Security and Sensing 2012

Baltimore, MD

05-08 to 05-10-2012

Vision Show

Boston, MA

More trade fairs