SCHOTT North America
|
Dental Applications Faceplates
Fused Fiber Optic Faceplates
|
Image Inverters; Step Plates; Radius Plates; Strip Plates; Hydrogen-fired Plates
SCHOTT's Fiber Optic Faceplates are used for high resolution, zero thickness image transfer in applications that include CCD coupling, CRT / LCD displays, image intensification, remote viewing, field flattening and x-ray imaging. In opto-electronic applications, faceplates are used as both input and output image intensifier windows.
All SCHOTT Faceplates are fabricated to customer-specific requirements. Typical customized shapes range from round to rectangular and vary in sizes up to 150 mm in diameter; typical element sizes range from as small as 4.0 µm up to 25 µm or larger; standard numerical
apertures (NA) is 1.0 Faceplates are manufactured to meet vacuum tube requirements. They are also manufactured with various coefficients of thermal expansion to meet customer's needs.
|
Small micron size elements
Radiation resistant materials
|
Radiation Resistant 47ARH Faceplates
SCHOTT Lighting and Imaging 47ARH Faceplates are produced using a core glass which substantially improves radiation resistance, yet retains the properties required for use as windows in image intensifier tubes and similar applications. Faceplates made with 47ARH material can
withstand exposures of up to 100 rads of x-radiation, without significant darkening.
|
General Specifications
|
|
Material
SCHOTT Standard 47
with or without EMA. Compatible with phosphors and photocathodes.
CTE 68 x 10-7/°C. Seals to Niromet 44 using Corning 7578 frit.
SCHOTT Standard 24
with or without EMA. Compatible with phosphors. CTE 68 x 10-7/°C.
Seals to Niromet 44 using Corning 7578 frit.
SCHOTT Standard 73
CTE 89 x 10-7/°C. Seals to G12 glass.
SCHOTT Standard 283
CTE 62 x 10-7/°C.
Fiber Size / Theoretical Resolution for standard materials
4.0 µm/ 144 lp/mm
6 µm/102 lp/mm
10 µm/ 50 lp/mm
25 µm/ 24 lp/mm
Numerical Aperture
1.0
Vacuum Integrity
Per customer specification
Material Quality
Chicken Wire, blemishes and distortions (gross & shear). Will quote customer requests.
Surface Quality
Polished surfaces are controlled by the scratch/dig tolerance
of MIL-O-13830A and meet a 20/10 scratch/dig tolerance.
Surface Flatness
Will quote customer requests.
|
Typical Faceplate Specification
|
Glass Type
Typical Performance Parameters |
47A |
283C |
73A |
24A |
24 |
| Element Size(um)/ Resolution (lp/mm) |
6/102 |
6/102 |
6/102 |
6/102 |
6/102 |
| Numerical Aperture |
1.0 |
1.0 |
1.0 |
1.0 |
1.0 |
| Stray Light Control (EMA) |
Yes |
No |
Yes |
Yes |
No |
Collimated Transmission White Light:
3 mm Thick
10 mm Thick
|
72
70 |
81
78 |
68
62 |
65
58 |
85
44 |
Lambertian Transmission
3 mm Thick
10 mm Thick
|
64
60 |
79
76 |
60
54 |
59
53 |
85
44 |
| Coefficient of Thermal Expansion (x 10-7/°C) |
68 |
59 |
89
94 |
68 |
68 |
| Phosphor Compatible |
Yes |
Yes |
Yes |
Yes |
Yes |
|