Thin Layers – but very effective

With the PICVD technique, chemical reactants are deposited onto the inner surface of the containers. The results are either SiO2 layers that reduce ion leaching or hydrophobic coatings that offer advantages, such as improving emptying or the lyophilization process with medications.