SCHOTT Microarray Solutions offers two different types of slides with three dimensional coating. The slides are especially developed for protein applications but also suitable for DNA applications.








The following table should help you to find the appropriate product for your specific application.

Nexterion® Slide H Nexterion® Slide P
Active immobilisation chemistry NHS ester NHS ester
Spot diameter (split pins, SMP3)
Nexterion® Spot PB
50% DMSO, borate pH 8,0

120 µm
50µm

160 µm
90µm
High hydrophobicity +++ +
High Hydrophilicity + +++
Low unspecific binding +++ ++++
Signal Intensity +++ +++
Sensitivity +++ ++++
Support of protein structure/cell growth ++ +++


Contact

Microarray Solutions
SCHOTT North America Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA
 +1 -502-657-4411
 +1 -502-966-4976
E-mail
More contacts
Trade Fairs & Events

04-17 to 04-21-2010

AACR 101st Annual Meeting 2010

Washington, DC

04-18 to 04-21-2010

AACR 101st Annual Meeting

Washington, DC

05-25 to 05-26-2010

Advances in Microarray Technology

Dublin

07-25 to 07-29-2010

AACC Annual Meeting 2010

Anaheim, CA

More trade fairs