BOROFLOAT® 33 (NEXTERION® Glass B)

BOROFLOAT® 33 is a borosilicate glass produced with a microfloat process by melting the purest raw materials. It is one of the basic materials for the NEXTERION® coated and uncoated substrates.

The manufacturing process used for this glass type, resulting in a pristine, fire-polished surface that can be used without any additional polishing. BOROFLOAT® 33 is a highly chemical resistant material with excellent transmission, low fluorescence, exceptional flatness and tight geometric properties.

Manufactured using standardized processes and running a stringent quality control system, BOROFLOAT® 33 is the perfect material to be used for coated substrates. The uncoated type of this glass is available exclusively cleanroom cleaned (ISO class 5) and will be offered in standard as well as in custom formats.
  • Chemical and thermal Stability
    BOROFLOAT® 33 glass exhibits excellent chemical stability and durability. The glass provides an inert support for biomolecule immobilisation and hybridisation, and does not leach alkali ions over time.
    A particularly low coefficient of thermal expansion is what makes BOROFLOAT® glass remarkably resistant to high temperature levels. The glass is proven to stand up to high and fluctuating temperatures.
 
  • Fluorescence
    The extremely low fluorescence of the glass offers exceptionally low background signals for all fluorescence detection methods, thereby maximizing the signal-to-background ratios.
 
  • Flatness
    Exceptional flatness, tight thickness tolerances.
 
  • Roughness
    ≤1 nm RMS
     
  • Cleaning
    All NEXTERION® substrates are cleaned using an automated ultrasonic cleaning line using multiple wash steps of varying pH levels, rinse steps and final drying stage.
 
  • Packaging
    After cleaning, the substrates will be either coated or, in the case of uncleaned substrates, packed up in plastic storage boxes which are sealed in air-tight laminated foil pouches under inert atmosphere in an ISO class 5 (Class 100) clean room. The glass can be used without any additional cleaning step.
Exhibitions & Events
05.
June
Exhibition 5th Workshop Microarrays: Basics, Production and Processing, Zurich, Switzerland, 06-05 to 06-06-2018
05.
June
Exhibition Lab-on-a-Chip and Microfluidics Europe 2018, Rotterdam, Netherlands, 06-05 to 06-06-2018
01.
October
Exhibition Lab-on-a-Chip and Microfluidics World Congress 2018, Coronado Island, USA, 10-01 to 10-03-2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.