Home Help Sitemap Locations
print this page  email this page
Home Advanced Optics Filter
SCHOTT North America

Advanced Optics Home
Advanced Optics Home
Our Products
Aspherical Lenses
Calcium fluoride (Lithography)
Coating
Contrast Enhancement Filters
Cylindrical Lenses
DWDM Substrates
Fast Axis Collimation (FAC) Micro-Lenses
Fiber Rods
Fused Silica (Lithography)
Glass Filters
Grin Lenses
Instrument Glasses
Interference Filters
Laser Glass
Machined Blanks
Materials for Precision Molding
Molded Aspherical Lenses
Mounting & Assembling
Optical Glass
Plane Parallel Substrates
Precision Gobs
Pressings
Zerodur®

Projects
Grantecan Project
Exploring Space
Neutron Science

Order online
Order Products
Quote Requests

Glass Filter

Product Information



Colored and filter glass stands out due to its selective absorption in the visible wavelength range. The filters appear to be colored if their filter effect lies within the visible light spectrum.

SCHOTT, one of the leading filter glass manufacturers with a product range equalled by no other manufacturer world-wide, can provide virtually any size, shape and quality required by the customer. As series supplier, our expertise is available to our customers at all times and we help find the optimal solution to your filter problem.

Our range of glass filters with more than 60 types includes the following filter types in the visible wavelength range from 200 nm upwards:

  • Band pass filters, which allow required ranges to pass through selectively
  • Long pass filters, which block unwanted shorter wave ranges
  • Short pass filters, which block unwanted longer wave ranges
  • Neutral density filters, which have a virtually constant transparency especially in the visible range
  • Conversion filters, which due to their spectral range increase or reduce the color temperature of radiation sources
      Please also take a look at our Internet pages Contrast Enhancement Filter
      und Interferencefilter.


Our filters are divided into the following groups:

UG Black and blue glass which permits the transmission of UV light
BG Blue, blue-green and band glass
VG Green glass
GG Yellow glass which permits IR light transmission
OG Orange glass which permits IR light transmission
RG Red and black glass which permits IR light transmission
NG Neutral glass with virtually constant radiation weakening in the visible range
N-WG Colorless glass with different cut-off positions in the UV range and which allows IR and visible light transmission
KG Virtually colorless glass with high transmission of visible light and absorption of radiation in the IR range
FG Blue and brown colored glass (conversion glass)


33855_infobl_bg50_v3.pdf New Development BG 50 Color Compensating Filter
33855_infobl_bg55_v3.pdf New Development BG 55 Color Compensating Filter
Applications

Optical glass filters are used in a host of different applications. Optical glass filters are significant components in industrial measurement, control and regulation technology through analytical measuring methods in production, research and development all the way to environment protection and medicine with which to permit or block the transmission of specific spectral ranges. We have listed a number of possible applications below:

  • "Keep it out of your eyes "

  • KG3 and KG5, which stand out because of their high transmission of visible light and effective absorption in the infra-red range (especially 1064 nm for Nd:YAG-Laser) are used as components in protective glasses and windows for lasers.

  • "Cool light in the operating theatre" – KG1 and KG3 in operating lights

  • The extensive colour neutrality of our heat absorption filters KG1 – KG5 in the visible spectrum prevents colours being falsified in the operating area.

  • "Seeing in the dark"

  • Spotlights which are equipped with RG filters only allow IR radiation to be transmitted and when in operation appear black to the observer. Together with cameras sensitive to infra-red radiation, they can be used for monitoring tasks without being noticed.


    Materials

    Forms of Supply

  • Polished filter:

  • Filters are available as polished plates or round discs with processed edges. Upon request, they are available thermally strengthened and / or with a protective / antireflection coating.

  • Filter glass prepared:

  •     - With processed edges
          Rectangular plates and round discs with matt surface and processed edges.

        - Edges not processed
          Rectangular plates and round discs with matt surfaces and edges not processed.

  • Standard formats with non-processed edges:

  • Plate sizes 165 mm x 165 mm + 3-0 mm
    Plate thickness 3.5 mm ± 0.5 mm and 4.5 mm ± 0.5 mm
    (available within a short period of time)


    Specifications

    Dimensions
    Minimum thickness
    from 1 mm - 480 mm
    0.1 mm
    TolerancesUp to 0.001 mm
    Surface qualityUp to P 4 in compl. with DIN ISO 10110


    Upon request, we can produce any size and thickness required within the framework of the maximum size permitted by the type of glass required.

    Further information is available from our data sheets and glass filter catalogue.


    Quality Assurance

    Filter glass production is subjected to continuous quality control with continuous documentation of the respective production steps. As far as is permitted by the transparency of our glass, the interior quality of our glass is checked for bubbles, smears etc. Powerful top quality measuring devices are then used to perform a final check on the filters.



    For more information please contact:

    Advanced Optics
    SCHOTT North America, Inc.
    400 York Avenue
    Duryea, PA 18642
    USA
    Phone: + 1 (570) 457-7485
    Fax: + 1 (570) 457-6960
     E-mail
    www.us.schott.com/optics_devices/

    Business Contact
    Advanced Optics
    SCHOTT North America, Inc.

    400 York Avenue
    Duryea, PA 18642
    USA

     + 1 (570) 457-7485
     + 1 (570) 457-6960
     E-mail
    more contacts 

    Fairs & Events

    06-16 to 06-20-2008
    Eurosatory
    Paris


    more fairs 

    back to overview Top
    ©2008 SCHOTT North America, Inc. - Legal
    Home