Prefillable polymer syringes

SCHOTT TopPac® prefillable syringes

SCHOTT TopPac
SCHOTT Popup

Sterile prefillable syringes made of advanced cyclic olefin copolymer (COC).

  • Syringes available with luer cone and integrated luer lock
  • Automated assembly technology with in-line process control
  • Precision molding
  • Clean room packaging
  • DMF 18416