The Beauty of Safety: SCHOTT PYRAN® Fire-Rated Glass Ceramic


PYRAN® Platinum is the best fire-rated glass you’ve ever seen


SCHOTT announces a revolutionary development with its SCHOTT PYRAN® Platinum fire-rated glass-ceramic. Because it is produced by an innovative patented process, PYRAN® Platinum fire-rated glass-ceramic offers stunning optical quality with superior clarity and virtually no distortion. It was designed especially for the North American market for use in fire-rated doors and windows.

The new SCHOTT PYRAN® Platinum line is UL classified and passes the hose stream test. It is readily available through our distributors.

Hose Stream Test






SCHOTT's dedicated development team has made sure that PYRAN® Platinum is environmentally friendly.

It is the only fire-rated glass-ceramic that is made without the use of hazardous heavy metals antimony or arsenic.


PYRAN® Platinum Fire-Rated Glass-Ceramics Listings Table


PYRAN® glass-ceramic type
Rating
(minutes)
Location
Max. exposed area of glazing
(in2)
Max. width of exposed glazing
(inches)
Max. height exposed glazing
(inches)
Min. depth of groove
(inches)
Impact Safety Rated
PYRAN® Platinum
Up to 90
Other than doors
3,422
(23.7 ft2)
76
76
5/8
No
PYRAN® Platinum F
Up to 90
Doors non-temp rise
2,736
(19 ft2)
36
76
5/8
Yes
Up to 180
Doors temp rise and non-temp rise
100
(0.69 ft2)
12
33
1/2
Yes
Up to 90
Other than doors
3,422
(23.7 ft2)
76
76
5/8
Yes
PYRAN® Platinum L
Up to 90
Doors non-temp rise
2,736
(19 ft2)
36
75
5/8
Yes
Up to 180
Doors temp rise and non-temp rise
100
(0.69 ft2)
12
75
1/2
Yes
Up to 90
Other than doors
3,143
(21.8 ft2)
75
75
5/8
Yes


Contact

Home Tech
SCHOTT North America, Inc.

5530 Shepherdsville Road
Louisville, KY 40228
USA
 +1 (502) 657-4439
 +1 (502) 966-4976
E-mail
Directions
More contacts
Trade Fairs & Events

09-11 to 09-14-2012

Construct 2012

Phoenix, AZ

11-14 to 11-16-2012

GreenBuild

San Francisco, CA

More trade fairs