SCHOTT PYRAN® Platinum Fire-Rated Glass-Ceramic
PRODUCT INFORMATION
Description
PYRAN® Platinum is a fire-protection rated and impact safety-rated glazing material made from a transparent glass-ceramic with a thickness of 3/16" (5 mm).
It is intended for use in non-impact, safety-rated locations such as transoms and windows with fire-rating requirements up to 90 minutes.
|
 |
|
|
|
|
 |
 |
|
|
|
- Fire-rated up to 90 minutes with the required hose stream test
- Specially floated glass-ceramic
- Transparent and wireless
- Withstands thermal shock
- Suited for use with standard fire-rated frames with the same rating
- Conforms to positive pressure test standards
- Environmentally-frinedly glass-ceramic; produced without the use of toxins
- Can be used to construct insulated glazing units
|
- Thickness: 3/16" (5 mm)
- Weight: 2.5 lbs/ft²
- True color rendition
- Surface finish: Nearly invisible micro-structure
- Maximum sheet sizes: Approximately 43" x 77"
- Impact rating: None (For applications requiring an impact-rated material SCHOTT offers PYRAN® Platinum F and PYRAN® Platinum L products)
|
Rating |
Location |
Max. exposed area of glazing (in²) |
Max. width of exposed glazing (in) |
Max. height of exposed glazing (in) |
Min. depth of grrove (in) |
| Up to 90 min |
Other than Doors |
3,422 (23.7 ft²) |
76 |
76 |
5/8 |
|
Classified and labeled by Underwriters Laboratories, Inc. for the United
States and Canada with File-No. R22036. All fire tests performed in
accordance with UL 9, UL 10C, UBC 7-2 (1997), UBC 7-4 (1997), NFPA
257, NFPA 80, ASTM E2010-01, ASTM E2074-00, and ULC CAN4-S106.p>
Note: This product is not considered a barrier to radiant heat and has not met the ASTM E-119 or UL 263 test standards.
All listing information is subject to change. The current listing can be accessed in the UL directory under
file #R22036 or upon request from SCHOTT.
For special component requirements, contact SCHOTT North America, Inc., 5530 Shepherdsville Road, Louisville, KY 40228 or phone (502) 657-4417.
|
After cutting, each lite of PYRAN® Platinum fire-rated glass-ceramic shall
be permanently labeled according to code requirements with product
and manufacturer’s name, mark from the authorized testing agency, fire
rating, etc.
|
PYRAN® Platinum fire-rated glass-ceramic should be handled with care during transportation, storage, inspection, and installation. It should be
stored in dry conditions only and needs to be stacked upright or at a
slight angle. In addition, the panels must be separated by an appropriate
material, such as soft pads made of cork and the bottom edge must be
supported along its entire length.
|
PYRAN® Platinum shall only be installed into fire-rated frame and window
assemblies carrying the same rating. Each PYRAN® Platinum panel should be inspected carefully before installation, and any pieces with visible edge or surface damage should be sorted out. All glazing components and the stop height must be chosen according to the PYRAN® Platinum UL classification. The panel must be placed on calcium silicate or hardwood setting blocks and glazed using PYRAN® Platinum classified glazing tape, such as closed cell PVC, Fiberfrax tape or Pemko FG3000S90. The installation of the framed unit must comply with the frame supplier's instructions.
PYRAN® Platinum is a specially developed glass-ceramic, that fulfills the fire protection rating requirements. The production process may create certain optical imperfections, such as bubbles or knots. Since these do not generally impair the transparency or the technical performance of the glass-ceramic, they do not represent cause for rejection or replacement.
|
To maintain the aesthetics, it is important to keep the panel clean. A soft,
clean, non-abrasive cloth and a mild soap, detergent, or non-abrasive
window cleaning solution is suitable for cleaning. After cleaning, rinse
immediately with clean water and remove any excess water from the
panel surface. Also, do not allow any metal or hard parts of the cleaning
equipment to come in contact with the panel surface.
|
|