SCHOTT North America
|
SCHOTT PYRAN® Platinum L Fire- and Safety-Rated Glass-Ceramic
Description
PYRAN® Platinum L is a fire-protection rated and impact- safety rated glazing material with a thickness of approximately 3/8" (9 mm), a laminated glass-ceramic with a transparent appearance. It is intended for use in safety-rated locations such as door lites, transoms or sidelites, and windows with fire-rating requirements up to 90 minutes (doors: up to 3 hours).
|
 |
|
|
|
|
 |
 |
|
|
|
- Fire-rated up to 90 minutes (up to 180 minutes in doors) with required
hose stream test
- Specially floated glass-ceramic
- Transparent and wireless
- Withstands thermal shock
- Approved for use with any fire-rated frame
- Conforms to positive pressure test standards
- Environmentally-friendly glass-ceramic; produced without hazardous
heavy metals arsenic and antimony
- Cradle to Cradle® Certified Silver by MBDC
– Meets LEED Innovation in Design requirements
– Qualifies for Environmentally Preferred Purchasing Program (EPP)
- Can be used to construct insulated glazing units
- Can be lightly sandblasted or delivered with surface-applied opacity film
- Available locally throughout North America
|
- Thickness: 3/8" (9 mm)
- Weight: 4.0 lbs/ft²
- Clear; No amber tint
- Surface finish: Float glass quality
- Maximum sheet sizes: Approximately 43" x 77"
- Impact rating: ANSI Z97.1 (Class A) and CPSC 16CFR1201 (Cat. I and II)
- STC rating: approximately 36dB
|
Rating |
Location |
Max. exposed area of glazing (in²) |
Max. width of exposed glazing (in) |
Max. height of exposed glazing (in) |
Min. depth of groove in) |
Groove Width (in) |
Building Code Marking |
| Up to 90 min |
Doors Non-Temp Rise |
2,736 (19 ft²) |
36 |
75 |
5/8 |
5/8, 1/2 |
D-H-HT-90 |
| Up to 180 min |
Doors Temp Rise and Non-Temp Rise |
100 (0.69 ft²) |
12 |
33 |
1/2 |
5/8 |
D-H-NT-180 |
| Up to 90 min |
Transom lites,
sidelites, windows |
3,143 (21.8 ft²) |
75 |
76 |
5/8 |
5/8 |
OH-90 |
|
Classified and labeled by Underwriters Laboratories, Inc. for the United States and Canada under File #R22036.
All fire tests performed in accordance with UL 9, UL 10B, UL10C, UBC 7-2 (1997), UBC 7-4 (1997), NFPA 252,NFPA 257, NFPA 80, ULC Can4-5104, and ULC CAN4-5106.
Note: This product is not considered a barrier to radiant heat and has not met the ASTM E-119 or UL 263 test standards.
All listing information is subject to change. The current listing can be accessed in the UL directory under File #R22036 or upon request from SCHOTT.
For additional information, contact SCHOTT North America, Inc., 5530 Shepherdsville Road, Louisville, KY 40228 or phone (502) 657-4417.
|
After cutting, each lite of PYRAN® Platinum L fire- and safety-rated glass-ceramic shall
be permanently labeled according to code requirements with product and manufacturer’s name, UL certification mark, fire rating, etc.
|
PYRAN® Platinum L fire- and safety-rated glass-ceramic should be handled with care during transportation, storage, inspection, and installation. It should be
stored in dry conditions only and needs to be stacked upright or at a
slight angle. In addition, the panels must be separated by an appropriate
material, such as soft pads made of cork and the bottom edge must be
supported along its entire length.
|
PYRAN® Platinum L shall only be installed into fire-rated frame and window
assemblies carrying the same rating. Each PYRAN® Platinum L panel should be inspected carefully before installation, and any pieces with visible edge or surface damage should be sorted out. All glazing components and the stop height must be chosen according to the PYRAN® Platinum L UL classification. The panel must be placed on calcium silicate or hardwood setting blocks and glazed using PYRAN® Platinum L classified glazing tape, such as closed cell PVC, Fiberfrax tape or Pemko FG3000S90. The installation of the framed unit must comply with the frame supplier's.
PYRAN® Platinum L is a specially developed glass-ceramic, that fulfills the fire protection rating requirements. The production process may create certain optical imperfections, such as bubbles or knots. Since these do not generally impair the transparency or the technical performance of the glass-ceramic, they do not represent cause for rejection or replacement.
|
To maintain the aesthetics, it is important to keep the panel clean. A soft,
clean, non-abrasive cloth and a mild soap, detergent, or non-abrasive
window cleaning solution is suitable for cleaning. After cleaning, rinse
immediately with clean water and remove any excess water from the
panel surface. Also, do not allow any metal or hard parts of the cleaning
equipment to come in contact with the panel surface.
|
PYRAN® Platinum L Data SheetPYRAN® Platinum L Specifications (in MS Word) - Section 08 81 00 in CSI MasterFormat
|
|