Materials

The following glass types are available to produce the Glass Wafer & Substrates according to your requests:

  • BOROFLOAT® 33 borosilicate glass
  • Fused Silica
  • D 263 T® eco borosilicate glass
  • AF 32® eco aluminoborosilicate glass
  • B 270® low-iron crown glass


Main characteristics of BOROFLOAT® 33 borosilicate glass:

  • Low coefficient of thermal expansion -- close to silicon (a20°C – 300°C = 3.25 x 10–6 K–1)
  • Excellent transparency
  • High thermal resistance
  • High resistance to chemical solvents
  • Available in various thickness: 0.7 mm; 1.1 to 7.5 mm
  • Suitable for anodic bonding

    Click here for more information about BOROFLOAT® borosilicate glass.

  • Main characteristics of D 263 T® eco borosilicate glass:

    • Coefficient of thermal expansion matches with metals for hermetic sealing (a20°C – 300°C = 7.2 x 10–6 K–1)
    • High temperature resistance
    • High luminous transmission
    • Stable against sunlight and heat
    • Flexibility is similar to that of plastic
    • Smooth, fire-polished surface


    Click here for more information about D263 T eco borosilicate glass.

    Main characteristics of AF 32® eco:

  • Low coefficient of thermal expansion -- matches to silicon (a20°C – 300°C = 3.2 x 10–6 K–1)
  • Alkali-free in synthesis
  • Excellent transmission
  • High thermal resistance
  • Available in very thin thickness from 0.1 – 1.1 mm

    Click here for more informatin about AF 32® aluminoborosilicate glass.

  • Main characteristics of B 270®:

  • Thermal expansion coefficient at (a20°C – 300°C = 9.4 x 10–6 K–1)
  • Excellent transmission
  • High solarization stability
  • Available in many thickness from 0.8 – 10 mm

    Click here for more information about B 270® low-iron crown glass.

  • Contact

    Glass for Special Applications
    SCHOTT North America, Inc.

    400 York Avenue
    Duryea, PA 18642
    USA
     + 1 (570) 457-7485
     + 1 (570) 457-6960
    E-mail
    Directions
    More contacts