CONTURAN® is an anti-reflective glass
with optical interference coatings between
50 nm and 100 nm thick
applied to both sides by dip coating.
In contrast to conventional, uncoated
glass CONTURAN® provides the best
view at all times. Use this innovative
special glass technology with crystalclear
competitive benefits for your
products.
Less reflection –
high transmission
See for yourself, with your own eyes,
the product benefits that CONTURAN®
can offer you compared to standard
float glass. Its reduced reflection and
resultant high light transmission guarantees
an unrestricted view.
Visual colour impression
In transmission the visual rating of
CONTURAN® is colour neutral.
CONTURAN® Standard and Magic
show a greenish tinge in the reflection.
A blue-violet anti-reflective coating
can, however, be supplied on request.
The reflection from CONTURAN® Grey
is basically blue-violet.
High chemical resistance
CONTURAN® has proved its chemical
resistance in a range of test methods.
Its anti-reflective coating has demonstrated
that it is resistant to drinks and
cockpit sprays. The Copper Accelerated
Acetic Acid-Salt Spray Testing has
confirmed its good resistance to
corrosion: no peeling off of coating
visable.
Further processing for
greater safety
CONTURAN® can be used in the form
of thermally toughened glass (for safety
glass 4 mm thick) or as laminated
safety glass CONTURAN® Protect. The
optical properties of the latter are the
same as for CONTURAN® Standard or
alternatively CONTURAN® Magic of
the same total thickness.