D 263® T eco

D 263® T

Applications



The resistive touch panels used for car navigation systems are built with D 263® T eco. A touch panel using thin glass instead of a plastic film is more resistant to operating environmental influences such as heat or humidity. Therefore the touch panels with D 263® T eco can meet the high requirements of the automotive industry for an extended life time.


D 263® T eco as cover glass in opto-caps for laser diodes. Due to its variety in thicknesses and its flatness it can be processed to meet the requirements even of the smallest parts in the electronics industry.


D 263® T eco is used as substrate glass for IR-cut off filters in camera modules for mobile phones. Due to its very smooth surface it can be coated without previous polishing. With D 263® T eco our customers are always enabled to lead the miniaturization progression trend toward thinner glass in the electronics industry without having to change the material.

Contact

Glass for Special Applications
SCHOTT North America, Inc.

400 York Avenue
Duryea, PA 18642
USA
 + 1 (570) 457-7485
 + 1 (570) 457-6960
E-mail
Directions
More contacts