Protection for light-sensitive exhibits

UVILEX™ 390 Z blocks ultraviolet radiation from artificial light sources. Consequently, organic materials can be exposed to radiation considerably longer.

UVILEX™ 390 Z:

Primarily used for shop windows and display areas. A noticable change in the appearance of the color of objects displayed behind UVILEX™ 390 Z is not to be expected (general color rendering index Ra≥98) Saves energy and provides cost-saving UV-protection (see table)

Example of use in practice
A garment made of fur is exposed to daylight at a luminance of 1,000 lux daylight. In this case the permissible exposure time without incurring any fading is about 300 hours. With a conventional tungsten halogen lamp double this exposure time (600 hours) is possible. By using UVILEX™ 390 Z the exposure time is increased by as much as four times, so that the fur can be exposed to light for a total of 1,200 hours. The exact exposure times can be calculated by using the multiplication factors indicated in the table, for which you can find the link below.table


Table to calculate exposure times

Contact

SCHOTT North America, Inc.
Corporate Office

555 Taxter Road
Elmsford, NY 10523
USA
 +1 (914)831-2200
 +1 (914)831-2201
E-mail
More contacts