SCHOTT SUPREMAX® 33 Rolled Borosilicate Glass Sheets

SCHOTT SUPREMAX® 33 is a multifunctional rolled borosilicate glass with unlimited applications. It is available in sheet form with a chemical composition identical to SCHOTT’s floated borosilicate glass BOROFLOAT® 33.

Features of SCHOTT SUPREMAX® 33 Rolled Borosilicate Glass include: 

  • Low thermal expansion technical flat glass (C.T.E.: 3.25 x 10-6 K-1)
  • High thermal resistance (long term up to 450° C, short term up to 500° C)
  • Excellent light transmission from UV to NIR
  • Low density (12% lighter than soda lime glass)
  • Excellent chemical durability
  • Available in wide thickness range (28.6 mm - 57.2 mm)