Type II "Durable Anti Reflection"

"Durable Anti Relfection Coating" for maximum transmission

  • Reduces glass surface reflection by about 80%1, showing a residual air/glass reflection of only about 0.8%
  • Reduces scratches by more than 65%2

Facts and Figures:

  Type II
(Durable Anti Reflection)
Bare chemically strengthened
alumino silicate glass
Scratch Resistance2 High
(>65% scratches reduced)
Good
Avg. Residual Reflection1
(air – glass)
Excellent
(~0.8 %)
Good
(~4 %)
Coating Visibility (color effect) Marginal
(e.g. blueish)
Neutral
(bare glass)
Easy to Clean durability Increased
(>4.000 cycles)
No
Easy to Clean
Breakage Strength3 Good Good

Detailed technical data can be provided upon request.




1 Comparison of average reflections on coated vs. uncoated chemically strengthened lumino silicate glass. Measured for single air – glass interface for the wavelength 400 – 700nm (relevant wavelength for the human eye)
2 Sandpaper scratch test applied. Chemically strengthened alumino-silicate glass coated compared to traditional uncoated chemically strengthened alumino-silicate cover glass
3 Compared with uncoated, strengthened alumino silicate glass. Tested with a “real usage ball drop test” (coating faced up) with sandpaper