D 263® M Cover Glass

empty
Colorless Borosilicate Glass for flawless Miscroscopy 

D 263® M is a colorless borosilicate glass that SCHOTT manufactures with the help of a special down-draw method. It is available from stock in various sheet sizes and thicknesses ranging from 0.1 mm to 0.21 mm.

D 263® M is the perfect choice as cover glass for microscopic analysis and meets the requirements specified in ISO 8255-1.

The chemical composition of D 263® M ensures valid and reliable research results due to its low auto-fluorescence and high chemical resistance.